Rayon (and) Glycerin (plant derived) (and) Aqua (and) Urea (and) Styrene/Acrylates Copolymer (and) Blue 1 Lake (and) CI 19140 (and) CI 77000
1.50
B
Cocamide DEA
Cocamide DEA
4.50
Procedure
In the main kettle, add the 50% of the total weigh of the water and the Carboxymethyl
cellulose, mix with constant agitation until the CMC is fully dispersed. Continue adding
the rest of the water and the CMC with constant agitation.
Add the rest of the ingredients from Phase A and mix until an homogeneous gel is
visible.
In a side kettle, weigh Phase B and mix with slow agitation to prevent foam formation.
Add Phase B in the main kettle and keep mixing with slow agitation until the gel is
completely homogeneous.